ASTM 410S is a low-carbon ferritic stainless steel offering good corrosion resistance, weldability, heat resistance, and dimensional stability. Available in cold rolled strip, hot rolled strip, and plate in annealed condition.
UNS S41008 | EN X6Cr13 | W.Nr. 1.4000
Available in Cold Rolled Strip, Hot Rolled Strip and Plate forms in Annealed condition, with thickness starting from 26GA [0.50mm] up to 6″ [150mm].
Corrosion resistance: ASTM 410S exhibits good resistance to atmospheric corrosion, organic acids, alkalis, and some inorganic acids. This makes it suitable for applications in chemical processing, food processing, and pharmaceutical industries.
Heat resistance: ASTM 410S can withstand high temperatures without significant loss of strength and oxidation resistance. It is suitable for applications in high-temperature environments, such as heat exchangers, furnace components, and automotive exhaust systems.
Low carbon content: ASTM 410S has a lower carbon content compared to other stainless steel grades, which helps to minimize the formation of chromium carbide precipitation during welding, reducing the risk of intergranular corrosion.
Weldability: ASTM 410S exhibits good weldability, allowing for easy fabrication and welding using common methods such as gas tungsten arc welding and shielded metal arc welding.
Dimensional stability: ASTM 410S maintains good dimensional stability, ensuring accurate and consistent performance over time.
Magnetic properties: ASTM 410S is a magnetic stainless steel, which can be advantageous in certain applications where magnetic properties are desired.
# 1 – Hot rolled annealed and descaled. Smooth decorative finish is not required.
# 2D – Dull finish produced by cold rolling, annealing and descaling.
# 2B – Smooth finish produced by cold rolling, annealing and descaling.
# BA – Bright annealed cold rolled and bright annealed.
# CBA – Course bright annealed cold rolled matte finish and bright anneal.
# 2 – Cold Rolled.
# 2BA – Smooth finish produced by cold rolling and bright annealing. A light pass using highly polished rolls produces a glossy finish.
Final chemical, mechanical properties, dimensions and tolerances are confirmed against the governing specification and purchase order.
| % | Carbon | Manganese | Silicon | Phosphorus | Sulfur | Chromium |
|---|---|---|---|---|---|---|
| Min. | - | - | - | - | - | 12.00 |
| Max. | 0.08 | 1.00 | 1.00 | 0.040 | 0.015 | 14.00 |
| - | Tensile Strength | Yield Strength | Elongation | Hardness |
|---|---|---|---|---|
| Min. | 58 ksi [400 MPa] | 33 ksi [230 MPa] | 19% | - |
| Max. | 87 ksi [600 MPa] | - | - | 88 HRB |
Material lists, drawings or heat requirements — our desk responds with a full RFQ within one business day.