Widely used in petrochemical and energy industries due to it’s resistance to abrasion and pressure. Our supply range starts from 1/4″ [6.35mm] OD up to 3″ [76.2mm]
Final chemical, mechanical properties, dimensions and tolerances are confirmed against the governing specification and purchase order.
| Steel Grade | C [%max] | Mn [%min-max] | P [%max] | S [%max] | Si [%max] | Cr [%min-max] | Mo [%max] |
|---|---|---|---|---|---|---|---|
| ASTM A179 | 0.18 | 0.27-0.63 | 0.035 | 0.035 | - | - | - |
| ASTM A192 | 0.18 | 0.27-0.63 | 0.035 | 0.035 | 0.025 | - | - |
| ASTM A334 Gr.1 | 0.30 | 0.40-1.06 | 0.025 | - | - | - | - |
| ASTM A334 Gr.3 | 0.19 | 0.37-0.64 | 0.025 | - | 0.18 | 3.20-3.80 | - |
| ASTM A334 Gr.6 | 0.30 | 0.39-1.06 | 0.025 | - | 0.10 | - | - |
| ASTM A199 / A213 T5 | 0.15 | 0.30-0.60 | 0.025 | 0.025 | 0.50 | 4.00-6.00 | 0.45-0.65 |
| ASTM A199 / A213 T9 | 0.15 | 0.30-0.60 | 0.025 | 0.025 | 0.25-1.00 | 8.00-10.00 | 1.00-1.50 |
| ASTM A199 / A213 T11 | 0.15 | 0.30-0.60 | 0.025 | 0.025 | 0.50-1.00- | 0.90-1.10 | 0.44-0.65 |
| Steel Grade | Yield Strength [min] | Tensile Strength [min] | Elongation [min] | Hardness [max] |
|---|---|---|---|---|
| ASTM A179 | 26 ksi (180 MPa) | 47 ksi (325 MPa) | 35 % | 72 HRB |
| ASTM A192 | 26 ksi (180 MPa) | 47 ksi (325 MPa) | 35 % | 77 HRB |
| ASTM A334 Gr. 1 | 30 ksi (205 MPa) | 55 ksi (380 MPa) | 35 % | 85 HRB |
| ASTM A334 Gr. 3 | 35 ksi (240 MPa) | 65 ksi (450 MPa) | 30 % | 90 HRB |
| ASTM A334 Gr. 6 | 35 ksi (240 MPa) | 60 ksi (415 MPa) | 30 % | 90 HRB |
| ASTM A199/ A213 T5 | 30 ksi (205 MPa) | 60 ksi (415 MPa) | 30 % | 85 HRB |
| ASTM A199/ A213 T9 | 30 ksi (205 MPa) | 60 ksi (415 MPa) | 30 % | 89 HRB |
| ASTM A199/ A213 T11 | 30 ksi (205 MPa) | 60 ksi (415 MPa) | 30 % | 85 HRB |
Material lists, drawings or heat requirements — our desk responds with a full RFQ within one business day.