321 is a titanium-stabilized chromium-nickel austenitic stainless steel grade available in plate, sheet, and strip forms for pressure vessels and general industrial applications. It offers excellent resistance to intergranular corrosion and good performance at elevated temperatures.

overView

Certified material. Clear documentation.

ASTM UNS WERKSTOFF NR. EN SAE AMS BS
A240 Grade 321 S32100 1.4541 X6CrNiTi18.10 30321 5689 S524
 

Austenitic stainless steel for high temperature environments.

Grades 321 and 347 are the basic austenitic 18/8 steel (Grade 304) stabilized by Titanium (321) or Niobium.

Combining high strength, resistance to scaling and phase stability with resistance to subsequent aqueous corrosion, 321 is suitable for applications in the temperature range of up to 1650°F [900°C]. As other austenitic grades, 321 have excellent forming and welding characteristics, are readily brake or roll formed and have outstanding welding characteristics. Post-weld annealing is not required.

The variant grade 321H is a modification of 321 with a higher carbon content, to provide improved high temperature strength.

Seamless Procurement, Quality & Logistics
Typical specification data

Technical reference

Final chemical, mechanical properties, dimensions and tolerances are confirmed against the governing specification and purchase order.

CHEMICAL PROPERTIES
CHEMICAL PROPERTIES Min % Max %
Carbon - 0.08
Manganese - 2.00
Phosphorus - 0.045
Sulfur - 0.030
Silicon - 0.75
Chromium 17.00 19.00
Nickel 9.00 12.00
Titanium - 0.70
Nitrogen - 0.10
MECHANICAL PROPERTIES
MECHANICAL PROPERTIES min.
Tensile Strength (MPa) 515
Tensile Strength (Ksi) 75
Yield Strength %0.2 (MPa) 205
Yield Strength %0.2 (Ksi) 30
Elongation % in 50mm (2") 40
Hardness Rockwell B (HRB) 95.00
Brinell (HB) 217